Spend the dough and get it coated. Those pipes are as rare as hens teeth. Paint, even 2000 degree paint, will blister and peel eventually, especially when the pipes are hot and you get caught in a rain storm. You'll be kickin yourself if you let that pipe rot through with rust.
I'm sure you can find a company close to you that does high temp ceramic coatings, but IMO Jet Hot is the best in the biz. I've seen pipes that were coated ten years ago that shine like they were just done.
-
What kind of pipe does he have there?Rob
1983 1100ES, 98' ST1100, 02' DR-Z400E and a few other 'bits and pieces'
Are you on the GSR Google Earth Map yet? http://www.thegsresources.com/_forum...d.php?t=170533
Comment
-
7981GS
-
I have heard nickel coatings are great too although I have no experience with them. A local shop will strip mine & coat it for $75.00. This is for the header & V & H megaphone.80 gs1100 16-v ported & polished, 1 mm oversize intake valves, 1150 carbs w/Dynojet stage 3, plus Bandit/gsxr upgrades
Comment
-
BassCliff gave me this site, check it out, might be what you want. http://www.jet-hot.com/sigpicMrBill Been a GSR member on and off since April 2002
1980 GS 750E Bought new in Feb of 1980
2015 CAN AM RTS
Stuff I've done to my bike:dancing: 1100E front end with new Sonic springs, 1100E swing arm conversion with new Progressive shocks installed, 530 sprockets/chain conversion, new SS brake lines, new brake pads. New SS fasteners through out. Rebuilt carbs, new EBC clutch springs and horn installed. New paint. Motor runs strong.
Comment
-
Coating would be best. I sandblasted mine earlier this spring and painted them with VHT Flameproof and have been through numerous rain storms without any problems. I had peeling and blistering before with the same paint before I sand blasted the pipes, so the preparation for the paint means a lot.http://www.thegsresources.com/_forum...ine=1440711157'78 GS1000E, Dyna-S ignition, Dyna Green Coils, K&N pods, Delkevic SS 4-1 exhaust, Dynojet Stage 3 jet kit, Russell SS Brake Lines, Progressive suspension, Compu-Fire series Regulator 55402 and Advmonster cree LED headlight conversion.
Comment
-
Originally posted by mrbill5491 View PostBassCliff gave me this site, check it out, might be what you want. http://www.jet-hot.com/No signature :(
Comment
-
Originally posted by TheCafeKid View PostSpend the dough and get it coated. Those pipes are as rare as hens teeth. Paint, even 2000 degree paint, will blister and peel eventually, especially when the pipes are hot and you get caught in a rain storm. You'll be kickin yourself if you let that pipe rot through with rust.
I'm sure you can find a company close to you that does high temp ceramic coatings, but IMO Jet Hot is the best in the biz. I've seen pipes that were coated ten years ago that shine like they were just done.
He should also repack the can with some coarse stainless steel.
Once that exhaust rusts out he is into a big problem finding something to replace, save for going back to a chrome V&H
Comment
-
Originally posted by posplayr View PostI agree, Gotta get that rust off and snd blasting is the only way. He might end up with some small holes since it is so blistered. I'm wondering if anybody ever rejetetd that bad boy when then added the Yoshi. It doesnt look like pods.
He should also repack the can with some coarse stainless steel.
Once that exhaust rusts out he is into a big problem finding something to replace, save for going back to a chrome V&H
Thanks guys,
TrevorNo signature :(
Comment
-
7981GS
VHT makes an ultra-hi temp paint that is rated to 2,000 degrees.
I highly recommend it if you are going to be painting.
The 1,200 degree stuff just doesn't last very long (2-4,000 miles)
Eric
Comment
-
Originally posted by trevor View PostSo I will sandblast and paint. I have heard ceramic coating is pricey. ?? Don't wanna spend a lot on that. And will look at re-packing the can too.
Thanks guys,
Trevor
I got mine blasted, cleaned and coated this spring, with a satin black ceramic coating for $225 USD
Bob T. ~~ Play the GSR weekly photo game: Pic of Week Game
'83 GS1100E ~ '24 Triumph Speed 400 ~ '01 TRIUMPH TT600 ~ '67 HONDA CUB
Comment
-
razor02097
X3 for getting it coated... I have never had success with header paints lasting. I've tried what the can says (which is clean the piece then spray 2 even coats then let dry), heavy coats, light coats, primers, bare metal, even heating the part up then spraying on 3 or 4 coats. Didn't matter if it was iron or steel... It never lasts more than a season before it rusts.
Comment
-
madjack57754
I've had jet-hot do 3 sets for me so far. Pleased with the finish and durability doesn't even begin to cover how I feel about thier product and service.
FYI If you have the pipes blasted locally before sending them to jet-hot you can save some money.